Pressure-Treated Lumber after water, smoke or contamination
Pressure-treatment introduces specified protective chemicals for defined decay/insect exposure use categories. Treatment chemistry, depth, retention, species and use classification matter. A board can still absorb water, swell, check, support surface soil/mold or have compromised fastening even if adequately decay-protected in its intended exposure. Cut/drilled surfaces can expose less protected wood; Preserved Wood/AWPA M4 guidance addresses approved field treatment. KDAT means kiln dried after treatment, not 'will never wet'.
What the inspection covers
USDA Forest Service FPL-GTR-275 reports untreated wood can develop biological deterioration when MC persists above ~20–25% with oxygen; initial wood decay spore germination can need >~29% in cited research. These are susceptibility bands rather than a claim a specific treated piece will rot at precisely 20%. The exact preservative protects against specified organisms/uses only, and legacy treated materials may require additional identification/handling controls. Assess dampness, fastener corrosion, physical section loss, preservative treatment stamp where visible and source.
Cleaning, drying and specialist work
Correct source, clean supported biological surface residue and dry sound accessible members; pressure-treated wood can be retained when structural integrity/fasteners are sound and treatment remains appropriate. Structural softness, significant section loss, failed connections, incorrect wet-use classification or unsafe chemical handling require qualified trade assessment/replacement. Record actual wood MC method and member IDs; do not treat a 'treated' label as clearance or automatically grind chemical-treated material without dust/worker protections.